Mechanical Properties Metric English Comments
Secant Modulus, MD 0.689 GPa
99.9 ksi
ASTM D 882 A
Total Finathene® 6450 HDPE film  (discontinued **)
Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin..
Secant Modulus, MD 0.689 GPa
99.9 ksi
ASTM D 882 A
Total 6410 HDPE Film Resin
Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw..