Mechanical Properties Metric English Comments
Secant Modulus, MD 0.410 GPa
59.5 ksi
ASTM D882
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin  (discontinued **)
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In..
Secant Modulus, MD 0.410 GPa
59.5 ksi
ASTM D882
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer.