Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, MD = 47.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.330 GPa
47.9 ksi
2% Secant, 2 mil; ASTM D882
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin
Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1..
Copyright © lookpolymers.com All Rights Reserved