Mechanical Properties Metric English Comments
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
M. Holland Company LD120 LDPE  (discontinued **)
Features: Good Processability, Medium Strength, Good ToughnessUses: Industrial Applications, Liners, Packaging, Shrink WrapProcessing Method: Blown FilmInformation provided by M. Holland.
Secant Modulus, MD 0.179 - 1.05 GPa
26.0 - 152 ksi
Average value: 0.427 GPa Grade Count:13
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 12C01G2 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 12C01G3 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: ..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 12C01G4 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 12C01G5 Clarity LLDPE
Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 16501F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 16501F4 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 16501F6 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets ..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 16501F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Secant Modulus, MD 0.179 GPa
26.0 ksi
ASTM D882
LyondellBasell Montell 16501F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Secant Modulus, MD 0.179 - 0.207 GPa
26.0 - 30.0 ksi
Average value: 0.201 GPa Grade Count:5
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..