Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.145 GPa | 21.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |