Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.103 - 1.38 GPa | 160.0 - 200 ksi | ASTM D882 |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |