Polymer Property : Secant Modulus, MD = 1.38 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 1.172 - 1.38 GPa
170.0 - 200 ksi
ASTM D882
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 2000 is a 2 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipmen..
Secant Modulus, MD 1.103 - 1.38 GPa
160.0 - 200 ksi
ASTM D882
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..