Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.600 GPa | 87.0 ksi | 0.05-1.05%; ISO 527-3 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |
|||
Secant Modulus, MD | 0.600 - 1.00 GPa | 87.0 - 145 ksi | Film |
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Secant Modulus, MD | 0.600 GPa | 87.0 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TN2005 EVA General Film Copolymer TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e.. |