Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 55.8 - 97.0 MPa | 8100 - 14100 psi | Average value: 80.9 MPa Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |