Polymer Property : Shear Strength = 8700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 40.0 - 60.0 MPa
5800 - 8700 psi
2D
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..
Shear Strength 55.0 - 60.0 MPa
7980 - 8700 psi
IS 867-1963
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..