Mechanical Properties Metric English Comments
Shear Strength 40.0 - 55.2 MPa
5800 - 8000 psi
Average value: 51.9 MPa Grade Count:18
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Shear Strength 40.0 MPa
5800 psi
0°, Short Beam
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2
Information provided by HexCel
Shear Strength 40.0 - 60.0 MPa
5800 - 8700 psi
2D
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Description: Exclusively for mechanical applications. Impact-resistant, resistant to mechanical wear, noise-reducing, low friction. Well suited for parts where there are high mechanical load and wea..
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronax MMMF PTFE Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin with PTFE (Teflon®) and a very fine cotton fabric. Exclusively for mechanical applications. Very good dry run properties. Well s..
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit AS Phenolic, Paper Reinforcement, Black, Sheets
Description: ESD-protection quality according to SP-method 2472, IEC 61340-5-1 and EN 100015-1. SP ESD Approval Certificate No. 230-01-0137. High mechanical properties at temperatures up to 120°CAp..
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected and lasting electrical properties despit..
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o..
Shear Strength 40.0 MPa
5800 psi
ASTM D732
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Shear Strength 40.0 MPa
5800 psi
Overlap, Aluminum, 60°C for 2 hrs; ASTM D1002
3M Scotch-Weld™ DP920 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i..