Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 50.3 MPa @Temperature 149 °C |
7300 psi @Temperature 300 °F |
|
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |