Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 7.888 MPa | 1144 psi | Lap |
Epoxy Technology EPO-TEK® CF6-2 High Temperature Epoxy Product Description: EPO-TEK® CF6-2 is a two component, high temperature and high Tg epoxy designed for fiber optic packaging. Advantages & Application Notes: The low viscosity nature allows for wi.. |