Polymer Property : Shear Strength = 64.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 64.0 MPa
9280 psi
ASTM D732
Unitika UNILATE® 1 PC PET
Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe..
Shear Strength 64.0 - 74.0 MPa
9280 - 10700 psi
2mm/min.; IS 867-1963
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..