Polymer Property : Shear Strength = 6240 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 43.0 MPa

@Temperature 93.0 °C
6240 psi

@Temperature 199 °F
Compression interlaminar
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric
Information provided by HexCel
Shear Strength 43.0 MPa

@Temperature 75.0 °C
6240 psi

@Temperature 167 °F
0º, ILSS (Short Beam), Wet; EN2563
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel