Polymer Property : Shear Strength = 59500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 410 MPa
59500 psi
Goodfellow Iron 90/Chromium 9/Molybdenum 1 Alloy
High Chromium heat resistant ferritic steel with good weldability. Used for boiler tubesInformation provided by Goodfellow.