Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 410 MPa | 59500 psi | |
Goodfellow Iron 90/Chromium 9/Molybdenum 1 Alloy High Chromium heat resistant ferritic steel with good weldability. Used for boiler tubesInformation provided by Goodfellow. |