Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 58.9 - 59.2 MPa | 8540 - 8590 psi | ASTM D732 |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |