Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 5300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 36.5 MPa

@Temperature 23.9 °C
5300 psi

@Temperature 75.0 °F
Interlaminar; Dry; Autoclave, 50psi, 90min; ASTM D2344
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring ..
Shear Strength 36.5 MPa
5300 psi
Overlap, Isopropyl Alcohol immersion, RT for 30 days
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 36.5 MPa

@Temperature 23.0 °C
5300 psi

@Temperature 73.4 °F
Aluminum Overlap
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
Shear Strength 36.5 MPa

@Temperature 204 °C
5300 psi

@Temperature 399 °F
Bond Line
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M
Copyright © lookpolymers.com All Rights Reserved