Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 36.5 MPa @Temperature 23.9 °C |
5300 psi @Temperature 75.0 °F |
Interlaminar; Dry; Autoclave, 50psi, 90min; ASTM D2344 |
Park Electrochemical Nelcote® F-529 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-529 is a non-halogenated phenolic resin designed specifically for use in aircraft and mass-transit interior laminate and sandwich panels. F-529 was formulated for applications requiring .. |
|||
Shear Strength | 36.5 MPa | 5300 psi | Overlap, Isopropyl Alcohol immersion, RT for 30 days |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 36.5 MPa @Temperature 23.0 °C |
5300 psi @Temperature 73.4 °F |
Aluminum Overlap |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Shear Strength | 36.5 MPa @Temperature 204 °C |
5300 psi @Temperature 399 °F |
Bond Line |
3M Scotch-Weld™ EC-2086 Structural Adhesive 3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M |