Mechanical Properties Metric English Comments
Shear Strength 41.4 - 48.3 MPa
6000 - 7000 psi
ASTM D732
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Shear Strength 41.4 - 48.3 MPa
6000 - 7000 psi
ASTM D732
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..