Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 41.4 MPa | 6000 psi | Cured, tensile |
Resin Technology Group DP031199-1 Cationic UV Cure Epoxy Adhesive DP031199-1 is an epoxy-based, low-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a strong, chemically resistant, lo.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Cured, tensile |
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive EN 239-2 is an epoxy-based, medium viscosity, cationic- curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resist.. |
|||
Shear Strength | 41.4 - 48.3 MPa | 6000 - 7000 psi | ASTM D732 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Shear Strength | 41.4 - 48.3 MPa | 6000 - 7000 psi | ASTM D732 |
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Shear Bond Holding Strength |
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â.. |
|||
Shear Strength | 41.4 MPa @Temperature 25.0 °C |
6000 psi @Temperature 77.0 °F |
Die |
Lord Adhesives Thermosetâ„¢ MD-150 Conductive Adhesive LORD Thermosetâ„¢ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing app.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Lengthwise; ASTM D3946 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | Perpendicular Shear Stress, Crosswise; ASTM D3946 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Shear Strength | 41.4 MPa | 6000 psi | ASTM D732 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |