Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 290 - 400 MPa | 42100 - 58000 psi | |
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello.. |