Mechanical Properties Metric English Comments
Shear Strength 29.0 MPa

@Temperature 23.0 °C
4210 psi

@Temperature 73.4 °F
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel