Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.79 MPa @Temperature 177 °C |
405 psi @Temperature 351 °F |
Etched Aluminum Overlap |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 2.79 MPa | 405 psi | with grain |
Pyrotek E-1 Board Structural Insulating Board E-1 is a high-temperature board designed to combine structural strength and high insulating value. Structural insulation panels made from E-1 can be painted. Fibers generated while cutting E-1 are .. |