Mechanical Properties Metric English Comments
Shear Strength 27.75 MPa
4025 psi
Overlap, Stainless Steel, Adhesive Failure
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 27.75 MPa
4025 psi
Overlap, Etched Aluminum tested after 1 week of Immersion in IPA
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..