Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 27.75 MPa | 4025 psi | Overlap, Stainless Steel, Adhesive Failure |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 27.75 MPa | 4025 psi | Overlap, Etched Aluminum tested after 1 week of Immersion in IPA |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |