Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 247.5 MPa | 35900 psi | Pin Double Shear Strength |
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%.. |