Polymer Property : Shear Strength = 247.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 247.5 MPa
35900 psi
Pin Double Shear Strength
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy
This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%..