Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.36 MPa @Temperature 75.0 °C, Time 1.21e+6 sec |
343 psi @Temperature 167 °F, Time 336 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Shear Strength | 2.36 MPa @Temperature 75.0 °C, Time 1.21e+6 sec |
343 psi @Temperature 167 °F, Time 336 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |