Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.00 - 32.0 MPa | 145 - 4640 psi | Average value: 11.2 MPa Grade Count:44 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Shear Strength | 24.0 - 32.0 MPa | 3480 - 4640 psi | |
Ritelok RT80 High Strength Retainer Anaerobic. High strength, high viscosity retainer for bonding rigid assemblies of all types. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |