Ritelok RT80 High Strength Retainer

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok RT80 High Strength Retainer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic. High strength, high viscosity retainer for bonding rigid assemblies of all types. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Physical Properties Metric English Comments
Viscosity 1250 - 2200 cP
1250 - 2200 cP
Mechanical Properties Metric English Comments
Shear Strength 24.0 - 32.0 MPa
3480 - 4640 psi
Descriptive Properties Value Comments
Maximum Gap Fill 0.4 mm