Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.65 MPa | 530 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 1/4-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 3.65 MPa | 530 psi | Lap Shear Strength; ASTM D1002 |
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Shear Strength | 3.65 MPa | 530 psi | silicone property; ASTM D1002 |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Shear Strength | 3.65 MPa | 530 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |