Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.7 MPa | 2270 psi | Tensile lap |
Abatron AboCast 8101-5/AboCure 8101-5 5-Minute Epoxy AboCast 8101-5/AboCure 8101-5 is a very-fast-hardening 2-component epoxy adhesive, casting, and patching compound. It is a thixotropic (Vaseline-like consistency) form of the 8012-9 System. It is tr.. |