Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8101-5/AboCure 8101-5 5-Minute Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8101-5/AboCure 8101-5 5-Minute Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 8101-5/AboCure 8101-5 is a very-fast-hardening 2-component epoxy adhesive, casting, and patching compound. It is a thixotropic (Vaseline-like consistency) form of the 8012-9 System. It is translucent, and clear in thin layers. It is used where 8012-9 would be too runny. It does not have the brittleness typical of conventional 5-minute epoxies. It also provides high resistance to weather, water, salt spray, alkalis, diluted acids, several fuels, solvents, and other chemicals. Unlike other epoxies, a thin layer of this compound does not need any longer to harden than a thick casting.
Physical Properties Metric English Comments
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
Mechanical Properties Metric English Comments
Hardness, Shore D 13

@Time 601 sec
13

@Time 0.167 hour
33

@Time 1800 sec
33

@Time 0.500 hour
60

@Time 3600 sec
60

@Time 1.00 hour
74

@Time 86400 sec
74

@Time 24.0 hour
Shear Strength 15.7 MPa
2270 psi
Tensile lap
Processing Properties Metric English Comments
Pot Life 5.0 min
5.0 min
Gel Time 5.00 min

@Thickness 1.27 mm
5.00 min

@Thickness 0.0500 in
Descriptive Properties Value Comments
Color Translucent
Parts by Weight (pbw) 100
AboCast 8101-5
100
AboCure 8101-5
Viscosity Vaseline-like
Copyright © lookpolymers.com All Rights Reserved