Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 21.0 MPa | 3050 psi | ASTM D732 |
Glastic BMC SLC-1000 Glass-Reinforced Polyester Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage. |
|||
Shear Strength | 21.0 MPa | 3050 psi | In-plane. ASTM D3914 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
Shear Strength | 21.0 MPa | 3050 psi | Overlap, IPA for 14 days, Cohesive Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 21.0 MPa | 3050 psi | Overlap, Etched Al, Anti-icing Fluid at RT for 7 days |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |