Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 14.1 MPa | 2050 psi | Overlap, Copper (1/16" thick), Cohesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 14.1 MPa | 2050 psi | Overlap, PVC, Substrate Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 14.1 MPa | 2050 psi | Overlap, CRS (1/32" thick), Adhesive Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 14.1 MPa | 2050 psi | Overlap, PVC, Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |