Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 2.00 MPa | >= 290 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP - 3/16 - 7.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 2.00 MPa | >= 290 psi | Plate Shear, L Direction, min, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Shear Strength | 2.00 MPa | 290 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 1/4-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 2.00 MPa | 290 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 2.00 MPa | 290 psi | Lap Shear Strength; ASTM D1002 |
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Shear Strength | 2.00 MPa | 290 psi | Lap; Product Property; ASTM D1002 |
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Shear Strength | 2.00 MPa | 290 psi | average; ISO 1922 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Shear Strength | 2.00 MPa @Temperature 49.0 °C |
290 psi @Temperature 120 °F |
Overlap |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |