Polymer Property : Shear Strength = 18300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 126 MPa
18300 psi
ASTM C273
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK
LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding.