Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 126 MPa | 18300 psi | ASTM C273 |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding. |