Mechanical Properties Metric English Comments
Shear Strength 12.25 MPa
1776 psi
Lap
Epoxy Technology EPO-TEK® E3035T-2 Electrically Conductive Epoxy
Product Description: EPO-TEK® E3035T-2 is a single component, silver-filled epoxy for semiconductor die attach, as well as SMD attach on hybrid circuits.Advantages & Application Notes: This epoxy c..