Polymer Property : Shear Strength = 1680 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 11.6 MPa
1680 psi
Lap
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy
Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of..