Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 11.2 MPa | 1630 psi | |
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation |