Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/IM7 GS Fiber: IM7 GS, UD, 150 g/m2Information provided by HexCel |