Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 105 MPa | 15300 psi | Axial; ASTM D732 |
Greene Tweed Arlon® 1163 PEEK, Glass Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | 105 MPa @Temperature 23.0 °C |
15200 psi @Temperature 73.4 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/IM7 GS Fiber: IM7 GS, UD, 150 g/m2Information provided by HexCel |