Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 8.729 MPa
1266 psi
Lap
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other..