Polymer Property : Shear Strength = 12.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.0827 - 3.45 MPa
12.0 - 500 psi
Average value: 0.658 MPa Grade Count:16
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Shear Strength 0.0827 MPa
12.0 psi
Neoprene Rubber, after 48 hrs at 23°C
3M Fastbond™ 49 Insulation Adhesive
3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and ..
Shear Strength 0.0827 MPa
12.0 psi
Overlap, Acrylic, 50% RH
3M PN8017 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.0827 MPa
12.0 psi
Overlap, Acrylic, 50% RH
3M PN8019 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.0827 MPa
12.0 psi
Overlap, Acrylic, 50% RH
3M PN8027 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.0827 MPa
12.0 psi
Overlap, Acrylic, 50% RH
3M PN8029 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..