Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.0827 - 3.45 MPa | 12.0 - 500 psi | Average value: 0.658 MPa Grade Count:16 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Shear Strength | 0.0827 MPa | 12.0 psi | Neoprene Rubber, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Shear Strength | 0.0827 MPa | 12.0 psi | Overlap, Acrylic, 50% RH |
3M PN8017 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.0827 MPa | 12.0 psi | Overlap, Acrylic, 50% RH |
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.0827 MPa | 12.0 psi | Overlap, Acrylic, 50% RH |
3M PN8027 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Shear Strength | 0.0827 MPa | 12.0 psi | Overlap, Acrylic, 50% RH |
3M PN8029 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |