Shear Strength 7.991 MPa
1159 psi
Lap
Epoxy Technology EPO-TEK® E3001-6 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & ..