Shear Strength 10.81 MPa
1568 psi
Lap
Epoxy Technology EPO-TEK® U300-2 Two Component Epoxy
Material Description: A two component epoxy designed for capillary underfill of semiconductor chips and SMDs. Long potlife, high Tg, and optical clarity are a few of its traits. NASA approved lo..